Blank Medal Materials: Zinc Alloy, Iron, Wooden Medal Blanks & Acrylic Compared

Written by the Badge Artisans production team · Last updated: 2026-10-13

A blank is only as good as the substrate under it. Zinc alloy, iron, wooden medal blanks and acrylic sheets arrive in different states and carry different weights. Each accepts different decoration, and the choice made at the order stage decides what is still possible six weeks later. We die-cast zinc alloy in house and buy the rest in, so we see all four from the production side. This guide compares them by the constraints that bind: thickness, freight, exposure and finish. The custom blank insert medals range is where our own zinc alloy bases start.

blank-medal-materials
blank-medal-materials

What we’ll cover

  • Why the substrate, not the event theme, drives a blank material decision
  • What each of the four materials actually is before decoration begins
  • The thickness envelope each substrate can hold without warping
  • Where material choice shows up on the freight invoice
  • How each substrate behaves outdoors, and what to fix on the purchase order
Blank medal bases laid out to show the material options available before decoration
Blank medal bases laid out to show the material options available before decoration

Why Blank Substrate Choice Is Really a Constraint Decision

Most material guides start with the event. That works when the question is what a finished medal should look like. The event-led view is covered properly in our guide to choosing the right medal material for your event. It stops working the moment the order is for an undecorated base, because a blank has to survive a production process before it ever reaches a podium.

Four constraints decide a blank material. They are the thickness the shape needs, the weight the freight can carry, the exposure the medal will face, and the decoration route the design depends on. Change any one and the material can change with it.

Zinc alloy runs at 6.7 g/cm³, iron at 7.8 g/cm³ and aluminium at 2.7 g/cm³. A shape cut in iron is roughly 16% heavier than the same shape in zinc alloy, and an aluminium version weighs less than half.

Comparison of zinc alloy, iron, copper and stainless steel as medal substrates
Comparison of zinc alloy, iron, copper and stainless steel as medal substrates

Zinc Alloy Medal Blanks: Cast Density, Thickness Range and a Plating Step Ahead

Zinc alloy is the substrate we make ourselves. Our own blank insert medals arrive cast, trimmed and polished, and then go through plating before they are finished. That is one more production step than wood or acrylic needs, and it is the step that decides the final surface. The reasoning behind that choice for race work is set out in our note on why die casting suits race medals.

The process runs on an 88-ton die-casting press. Molten zinc alloy enters the mould at around 385°C, and because the alloy flows well at that temperature it fills fine detail that stamped metal cannot reach. Our moulds can hold a raised or recessed metal contour down to 0.2mm. Grass texture, hair detail and thin logo strokes all come out of the die, not out of a printer.

Thickness is where zinc alloy blanks get specified wrongly most often. We recommend 3mm as the floor for a standard medal. A base under 2.5mm flexes in the hand, and flexing decoration eventually cracks. Once 3D relief is involved the floor rises to 4mm, and a medal wider than 70mm needs 4.5mm to stop a large flat face from warping.

Plating is not optional on a metal blank. We work to a minimum plating thickness of 3μm. The alkaline copper strike runs at least 500 seconds to cover the whole surface. The acid copper step that follows runs 20 to 60 minutes, depending on the target gloss. A thinner layer wears through at edges and raised detail and exposes the base metal within three to six months.

Zinc alloy is often described as the cheap option. On a per-kilo basis it is not — zinc alloy costs more than iron. The reason to choose it is plasticity, not price. Fine 3D relief, hollow shapes and irregular outlines are simply not available in stamped metal.

Raw zinc alloy material stock used for die-cast medal blanks
Raw zinc alloy material stock used for die-cast medal blanks

Iron Substrates: Stamped Relief, Extra Weight and a Rust Risk to Manage

Iron blanks are stamped from sheet rather than cast. That single difference explains most of their behaviour: they are cheaper per piece, harder to bend, and limited to flatter relief than a die-cast part.

Stamping has a thickness ceiling in the other direction. Iron above 4mm becomes difficult to press cleanly, so deep relief is not an option. A design that needs a steep 3D stack or an undercut belongs in zinc alloy, not iron.

The bigger issue is corrosion. Iron carries no corrosion resistance of its own. Every iron blank depends entirely on its plating to keep rust away, and a scratch that breaches the plating lets rust spread outward from that point. We will not recommend iron for a humid climate, a coastal event or a sea-freight programme that sits in a container for weeks.

Where iron does earn its place is a large, simple, flat shape at a volume where unit cost matters more than surface detail. A single-colour print or a flat enamel fill on a simple outline is a reasonable fit.

Iron medal blank produced at a lower unit cost than a die-cast alternative
Iron medal blank produced at a lower unit cost than a die-cast alternative

Wooden Medal Blanks: Grain Direction, Sealing and How Laser Responds

Wooden medal blanks are cut from sheet, not cast. Sheet stock runs 2mm to 7mm in the common range, and a multi-layer or wood-and-metal assembly can reach 11mm to 17mm. Wood takes no plating and no enamel, so the decoration routes are narrower than for metal.

Grain direction is the detail that catches buyers out. Laser engraving and cutting behave differently along the grain than across it, and a fine serif or a thin script line can blur where the grain runs with the stroke. Design checks that look fine on screen can fail on a birch blank. The practical fix is to keep engraved text above a certain stroke weight.

Sealing is the second variable. An unsealed wood blank absorbs moisture, swells slightly and can raise the grain around a laser mark. A sealed blank holds its surface and takes a cleaner edge. If the medals will be handled outdoors or stored in a damp room, sealing is worth specifying up front.

Wood is also the substrate that carries an eco story, which is why it keeps appearing in trail and parkrun style events. We supply wood components as part of mixed-material builds rather than as an in-house line, so the specification comes from the case record. One reference build combines a zinc alloy body with wood detail at 76 × 94 × 11mm in a black nickel finish. The wider picture on that substrate sits in our wooden running medals guide, and the marking side is covered in blank medals for engraving.

Laser engraving detail on a wooden medal blank showing how grain affects the mark
Laser engraving detail on a wooden medal blank showing how grain affects the mark

Acrylic Medal Blanks: Sheet Clarity, Edge Quality and Ink Anchoring

Acrylic is a sheet material, which makes it the lightest and the cheapest of the four in most specifications. Acrylic versions of a design typically land 30% to 50% below the zinc alloy equivalent, and the colour range is wider because the sheet itself can be tinted.

Decoration on acrylic is printing, not metalwork. UV printing and lamination are the standard routes, and the printed image sits on the surface rather than in a recess. That means there is no enamel fill and no plating colour to choose — the finish decision is a print decision.

Edge quality is where acrylic separates good from poor. A laser-cut edge can come away with a slight frost or a visible cut mark, and on a clear sheet that edge is part of the look. Polished or flame-treated edges cost more and read much better on a clear or transparent blank.

Acrylic also accepts structures the metals cannot. Sandwiched and floating constructions — a loose element suspended between two sheets — are a standard acrylic technique and a real point of difference.

Acrylic medal blank with a printed logo, showing sheet clarity and edge finish
Acrylic medal blank with a printed logo, showing sheet clarity and edge finish

Sublimation Medal Blanks: A Polymer Coating Rather Than a Cast Metal

What the trade calls sublimation medals blanks is not really a metal category at all. It is a coated substrate. Sublimation ink turns to gas under heat and bonds into a polymer layer on the surface, so the blank must carry a receptive coating before anything else happens.

That single requirement rules materials in and out. Raw zinc alloy takes no sublimation. Bare wood takes no sublimation. A coated metal sheet, a coated MDF panel and a coated acrylic sheet all do. The coating is applied when the blank is made, so it cannot be added later — if sublimation is the plan, the coating is the specification.

The trade-off matters. Sublimation produces full-colour, photographic results with no per-colour charge, which suits busy artwork with gradients. But the image sits in the coating rather than the metal, so the life of the print is the life of the coating.

Thickness Envelope: What Each Substrate Can Hold Without Distortion

Every material has a thickness band. Below it the blank flexes, above it the process stops working, and the shape you designed determines where in the band the order has to sit.

The floors matter more than the ceilings. Zinc alloy needs 3mm for a standard shape, 4mm once relief is stacked, and 4.5mm above 70mm across. Iron becomes hard to stamp cleanly past 4mm. Wood sheet runs 2mm to 7mm in the common range, with assemblies reaching higher. Acrylic follows sheet stock, so thickness is chosen from what the supplier holds rather than built up.

SubstratePractical thickness bandCeiling that bitesTypical failure below the floor
Zinc alloy (cast)3mm floor; 4mm with 3D relief; 4.5mm above 70mmCasting handles thick sections wellFlexes under 2.5mm, then cracks the decoration
Iron (stamped)Simple flat shapes onlyClean stamping gets difficult past 4mmBends at thin gauges, loses relief definition
Wood (sheet)2–7mm common; assemblies 11–17mmSheet stock availabilityUnsealed stock swells and raises grain
Acrylic (sheet)Sheet stock thicknessSheet stock availabilityThin sheet chips at a laser-cut edge

One rule crosses all four materials. Our minimum through-hole is 2mm, and above 2.5mm of thickness the hole has to get larger as the part gets thicker. A 3mm hole in a 3mm blank is fine. The same hole in a 5mm blank is a design change, and it has to be settled before the die is cut.

Reference chart covering medal size, thickness and weight specifications
Reference chart covering medal size, thickness and weight specifications

Freight Weight: Where Substrate Choice Shows Up on the Invoice

Freight is the cost line most buyers forget when they compare materials, and it is the one where substrate choice is felt hardest at volume. Sea freight is priced on weight and volume together, so a heavier substrate costs more to move even when the unit price is lower.

This is why 3mm became the international default for a standard medal. It is the thinnest section that still holds shape, and it keeps the shipping weight of a large order under control. A supplier who quotes 5mm as standard is adding freight cost as well as material cost.

Weight differences are easy to underestimate. Iron is about 16% denser than zinc alloy, so an identical shape weighs more. Aluminium at 2.7 g/cm³ is lighter again, at the cost of rigidity. For a 5,000-piece order the gap is worth calculating before the material is locked.

For a programme that repeats, the same weight logic sits behind our wholesale blank medals planning, where stock bases take the tooling line out of the repeat order.

Production and freight are separate clocks, and neither is a promise. Bulk production runs 15–18 days from receipt of payment. Freight then runs from dispatch, excluding customs. Express courier takes 5–7 days with a further 2–3 days in delays. Air freight takes 10–15 days, with 2–7 days added for remote addresses. Sea freight runs 25–35 days on a fast boat and 30–45 days on a slow one. Sea freight needs 2–3 months of planning. Freight is quoted at actual cost against the real shipment.

Packing options that determine the shipped volume of a blank medal order
Packing options that determine the shipped volume of a blank medal order

Outdoor Exposure: How Each Substrate Ages Across One Season

An indoor award and an outdoor race medal are different engineering problems. A blank that looks correct on a desk can fail on a course, usually through corrosion or coating wear.

Corrosion resistance separates the metals clearly. Zinc alloy does not rust, which is why it holds up in humid conditions. Brass and aluminium also resist corrosion well. Stainless steel is the strongest of the group. Iron is the outlier: it rusts, and it relies completely on its plating to prevent that.

Coating wear is the slower failure. A plating layer below 3μm wears through at edges and raised points first, and the base metal shows within three to six months of regular handling. Sweat accelerates the process on iron and speeds oxidation on thin gold layers. Direct sun fades painted colour over a long season.

SubstrateCorrosion behaviourDeformation resistanceOutdoor verdict
Zinc alloyDoes not rustFlexes below 2.5mmStrong choice for humid and coastal events
IronRusts; fully dependent on platingHard and stiffAvoid in humid, coastal or long-transit programmes
WoodDegrades if unsealedRigid in sheet formSealed stock only for outdoor use
AcrylicResists moisture; can crazeChips at thin edgesFine outdoors if the edge is protected
Plating finish options for outdoor medals, from antique to bright gold and silver
Plating finish options for outdoor medals, from antique to bright gold and silver

Writing the Substrate Spec: What to Lock Before Tooling Starts

A blank order fails most often on a field that was left open. Once a die is cut, the shape and the recess geometry are fixed for its life. The specification has to be complete before tooling begins, not after the first sample.

Six fields decide a blank order: material, thickness, finished size, the state the blank arrives in, the plating colour or coating, and the decoration route that follows. Leave any of them open and the quotation is a guess.

Artwork format is a frequent cause of delay. We work from AI, CDR, PDF or STL. A raster logo has to be converted to vector before it can be cut into a die, and the converted version will not match the original exactly. Comparing the vector proof against the original file side by side is the cheapest check in the whole process. Revisions beyond three are chargeable.

On a custom blank medals order the blank spec and the decoration spec are two separate documents, and both have to be signed off before the die is cut.

Tooling and quantity terms are worth confirming in the same pass. Minimum order is 100 pieces per shape. For an 80mm × 3mm soft enamel blank in 2–3 colours, a single-specification reference price is US$1.25–1.45 per piece with a US$125 tooling charge. That figure is one specification, not a general medal price — colour count, size, thickness, structure and non-standard plating combinations all move it. Moulds are retained for three years, and the tooling charge is refundable once an order passes 10,000 pieces.

Mould engraving in progress, the step that locks a blank's shape and recess geometry
Mould engraving in progress, the step that locks a blank’s shape and recess geometry

Blank Medal Base Material: Weight, Freight and Surface Finish

With the constraints mapped, the four substrates line up in a single view. The comparison below is not a ranking — each column describes what that material is good at and what it forces you to give up.

Zinc alloyIronWoodAcrylic
Density6.7 g/cm³7.8 g/cm³Light sheetLightest option
FormingDie-cast; fine 3D and hollow shapesStamped; flat relief onlyCut from sheetCut from sheet
Surface routePlating, then enamel or printPlating required, then print or enamelSealing, then laserUV print and lamination
CorrosionDoes not rustRusts without platingNeeds sealing outdoorsResists moisture
Relative costBaselineLower unit costMid, varies by stock30–50% below zinc alloy
Forces you to acceptA plating step and a heavier partRust risk and flatter designNo plating, no enamel, grain limitsNo enamel, edge quality varies

Reading the table is straightforward. If the design needs fine 3D relief, hollow detail or an undercut, the answer is zinc alloy. If the design is a large flat shape and unit cost leads, iron or acrylic will do it for less. If the event story is environmental, wood carries it. If the piece has to be light and colourful, acrylic wins on both counts.

Side-by-side comparison of zinc alloy, brass and iron medal blanks
Side-by-side comparison of zinc alloy, brass and iron medal blanks

Substrate Limits: Where a Material Forces a Design Rethink

Every material has a line the artwork cannot cross. Finding it before the design is signed off is far cheaper than finding it at the sample stage.

Zinc alloy is the most permissive of the four, but it is not unlimited. A raised or recessed metal contour cannot go below 0.2mm, because the die itself cannot be cut that fine. Colour fill needs more room than the contour: 0.3mm minimum width for soft enamel and 0.5mm for imitation hard enamel, which is thicker and needs more space to settle.

Iron forces the sharpest rethink. A design with deep relief, an undercut or a hollow centre simply is not available in stamped metal, and no amount of tooling budget changes that. Wood pushes back on fine line work, because grain fights thin strokes. Acrylic pushes back on anything that assumes a recess, because there is no recess to fill.

The most common design failure we see on a blank order is a proof that was approved on screen. Screen artwork has no thickness, no grain and no coating. A design that depends on hairline detail across a wood blank, or on enamel sitting in an acrylic recess, is only discovered at the sample stage.

When the material and the design genuinely conflict, the cheaper change is almost always the design. Redrawing a thin stroke or dropping an undercut costs a few hours. Changing the die costs the tooling charge again, and it restarts the whole production clock. If the whole range needs a different treatment, the custom medals overview shows how a blank-base programme fits against fully custom work.

Medal design sketch used to check detail weight against the chosen substrate
Medal design sketch used to check detail weight against the chosen substrate

Frequently Asked Questions

Start with the constraint, not the event. If the design needs fine 3D relief, hollow detail or an undercut, use zinc alloy — it is the only one of the four that die-casts those features. If the shape is large and flat and unit cost leads, iron or acrylic will do it for less. Choose wood for an environmental story, and acrylic when the piece has to be light and colourful.

Start with the constraint, not the event. If the design needs fine 3D relief, hollow detail or an undercut, use zinc alloy — it is the only one of the four that die-casts those features. If the shape is large and flat and unit cost leads, iron or acrylic will do it for less. Choose wood for an environmental story, and acrylic when the piece has to be light and colourful.

Start with the constraint, not the event. If the design needs fine 3D relief, hollow detail or an undercut, use zinc alloy — it is the only one of the four that die-casts those features. If the shape is large and flat and unit cost leads, iron or acrylic will do it for less. Choose wood for an environmental story, and acrylic when the piece has to be light and colourful.

Start with the constraint, not the event. If the design needs fine 3D relief, hollow detail or an undercut, use zinc alloy — it is the only one of the four that die-casts those features. If the shape is large and flat and unit cost leads, iron or acrylic will do it for less. Choose wood for an environmental story, and acrylic when the piece has to be light and colourful.

Start with the constraint, not the event. If the design needs fine 3D relief, hollow detail or an undercut, use zinc alloy — it is the only one of the four that die-casts those features. If the shape is large and flat and unit cost leads, iron or acrylic will do it for less. Choose wood for an environmental story, and acrylic when the piece has to be light and colourful.

Start with the constraint, not the event. If the design needs fine 3D relief, hollow detail or an undercut, use zinc alloy — it is the only one of the four that die-casts those features. If the shape is large and flat and unit cost leads, iron or acrylic will do it for less. Choose wood for an environmental story, and acrylic when the piece has to be light and colourful.